The said process has a finished product rate higher than 95% and a sprue and riser head system weight lower than 20 wt% of the casting.
所得铸件的成品率为95%以上,浇冒口系统重量占铸件重量的20%以下。
These loads are transferred through the riser to the well - head and casing system, causing fatigue at critical connectors and welds.
这些载荷通过立管传递到井口和套管,在连接和焊接处形成临界疲劳区。